MV Labs AG1040 AgSCN Silver thiocyanate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs AG1040 AgSCN Silver thiocyanate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 165.95 g/mol
165.95 g/mol
Descriptive Properties Value Comments
Assay 65% Ag
CAS Number 1701-93-5
Form White crystals
Purity 99.99%
Typical Impurities Check with Manufacturer