MV Labs AU1030 Au2S3 Gold(III) sulfide

Category Ceramic , Sulfide/Chalcogenide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs AU1030 Au2S3 Gold(III) sulfide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 426.07 g/mol
426.07 g/mol
Descriptive Properties Value Comments
Assay 92% Au
CAS Number 1303-61-3
Form Black powder
Purity 99.99%
Typical Impurities Ag = 4; Al, Cu, Ni, Pd < 1 ppm