MV Labs BA880 Ba(OH)2.8H2O Barium hydroxide hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs BA880 Ba(OH)2.8H2O Barium hydroxide hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 171.36 g/mol
171.36 g/mol
Descriptive Properties Value Comments
Assay 73% Ba
CAS Number 40226-30-0
Form White crystals
Purity 99.995%
Typical Impurities Na, Sr < 10 ppm