Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 266.54 g/mol
266.54 g/mol
Descriptive Properties Value Comments
Assay 43% Cd
CAS Number 89759-80-8
Form White powder
Purity 99.999%
Typical Impurities Cu, Fe, Zn < 1 ppm