MV Labs CR890 (NH4)2Cr2O7 Ammonium dichromate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CR890 (NH4)2Cr2O7 Ammonium dichromate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 252.1 g/mol
252.1 g/mol
Descriptive Properties Value Comments
Assay 41% Cr
CAS Number 7789-09-5
Form orange crystals
Purity 99.999%
Typical Impurities Na = 7; Ca = 2; Fe < 1 ppm