Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 371.7 g/mol
371.7 g/mol
Descriptive Properties Value Comments
Assay 42% Gd
CAS Number 13450-84-5
Form White crystals
Purity 99.999%
Typical Impurities Ca, Tb = 5; Eu = 1; other Rare Earths < 10 ND