MV Labs GE800 GeO2 Germanium(IV) oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs GE800 GeO2 Germanium(IV) oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 104.59 g/mol
104.59 g/mol
Descriptive Properties Value Comments
Assay 69% Ge
CAS Number 1310-53-8
Form White powder
Purity 99.999%
Typical Impurities Si = 3; Ca, Fe, Mg = 2 ppm