MV Labs HG400 HgCl2 Mercury(II) chloride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs HG400 HgCl2 Mercury(II) chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 271.5 g/mol
271.5 g/mol
Descriptive Properties Value Comments
Assay 74% Hg
CAS Number 10112-91-1
Form White powder
Purity 99.999%
Typical Impurities No trace impurities detected