MV Labs HG600 HgI2 Mercury(II) iodide

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs HG600 HgI2 Mercury(II) iodide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 454.4 g/mol
454.4 g/mol
Descriptive Properties Value Comments
Assay 44% Hg
CAS Number 7774-29-0
Form Orange powder
Purity 99.999%
Typical Impurities No trace impurities detected