Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 216.59 g/mol
216.59 g/mol
Descriptive Properties Value Comments
Assay 93% Hg
CAS Number 21908-53-2
Form Orange powder
Purity 99.999%
Typical Impurities No trace impurities detected