MV Labs IN100 In(C2H3O2)3·xH2O Indium(III) acetate hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs IN100 In(C2H3O2)3·xH2O Indium(III) acetate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 291.96 g/mol
291.96 g/mol
Descriptive Properties Value Comments
Assay 30% In
CAS Number 304671-64-5
Form White powder
Purity 99.999%
Typical Impurities Bi, Cu, Pb, Mg = 1 ppm