MV Labs IN800 In2O3 Indium(III) oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs IN800 In2O3 Indium(III) oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 277.64 g/mol
277.64 g/mol
Descriptive Properties Value Comments
Assay 83% In
CAS Number 1312-43-3
Form Yellow powder
Purity 99.999%
Typical Impurities Pb, Bi, Cd, Cu, Fe, Mg, Ni, Si < 1 ppm