MV Labs IR445 K2IrCl6 Potassium hexachloroiridate(IV)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs IR445 K2IrCl6 Potassium hexachloroiridate(IV).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 483.12 g/mol
483.12 g/mol
Descriptive Properties Value Comments
Assay 40% Ir
CAS Number 16920-56-2
Form Purple-black crystals
Purity 99.99%
Typical Impurities Rh, Na = 25; Pt < 10 ppm