Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 102.01 g/mol
102.01 g/mol
Descriptive Properties Value Comments
Assay 6.8% Li
CAS Number 6108-17-4
Form White powder
Purity 99.999%
Typical Impurities Fe, Na <1; Ca, Cr, K, Mg, Si < 0.5 ppm