MV Labs NA1040 Na2S2O3 ·3H2O Sodium thiosulfate pentahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs NA1040 Na2S2O3 ·3H2O Sodium thiosulfate pentahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 248.18 g/mol
248.18 g/mol
Descriptive Properties Value Comments
Assay 19% Na
CAS Number 10102-17-7
Form White powder
Purity 99.999%
Typical Impurities Check with Manufacturer