MV Labs PR900 PrPO4 Praseodymium(III) phosphate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs PR900 PrPO4 Praseodymium(III) phosphate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 235.88 g/mol
235.88 g/mol
Descriptive Properties Value Comments
CAS Number 14298-31-8
Form Green powder
Purity 99.99%
Typical Impurities Check with Manufacturer