MV Labs RE1030 Re2S7 Rhenium(VII) sulfide

Category Ceramic , Sulfide/Chalcogenide
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs RE1030 Re2S7 Rhenium(VII) sulfide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 596.85 g/mol
596.85 g/mol
Descriptive Properties Value Comments
Assay 62% Re
CAS Number 12038-67-4
Form Black powder
Purity 99.999%
Typical Impurities Fe < 3 ppm