Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs SM700 Sm(NO3)3·6H2O Samarium nitrate hexahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs SM700 Sm(NO3)3·6H2O Samarium nitrate hexahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 444.46 g/mol
444.46 g/mol
Descriptive Properties Value Comments
Assay 34% Sm
CAS Number 13759-83-6
Form Yellow crystals
Purity 99.999%
Typical Impurities Rare Earths < 10 ND; Ca = 3; Fe, Mg < 1 ppm
Users viewing this material also viewed the following: