MV Labs TA800 Ta2O5 Tantalum(V) oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs TA800 Ta2O5 Tantalum(V) oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 441.89 g/mol
441.89 g/mol
Descriptive Properties Value Comments
Assay 82% Ta
CAS Number 1314-61-0
Form White powder
Purity 99.99+%
Typical Impurities Nb < 12; Mg = 12 ppm