Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 346.07 g/mol
346.07 g/mol
Descriptive Properties Value Comments
CAS Number 34431-47-5
Form Off-white powder
Purity 99.999%
Typical Impurities Check with Manufacturer