Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs Y1000 Y2(SO4)3·8H2O Yttrium sulfate octahydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs Y1000 Y2(SO4)3·8H2O Yttrium sulfate octahydrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 610.12 g/mol
610.12 g/mol
Descriptive Properties Value Comments
Assay 29% Y
CAS Number 7446-33-5
Form White crystals
Purity 99.999%
Typical Impurities Si = 2; Ca, Cu, Fe, Na, Pb, Zn < 1 ppm; Rare Earths < 10 ND
Users viewing this material also viewed the following: