MV Labs YB810 Yb2O3 Ytterbium oxide

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs YB810 Yb2O3 Ytterbium oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 394.08 g/mol
394.08 g/mol
Descriptive Properties Value Comments
Assay 88% Yb
CAS Number 1314-37-0
Form White powder
Purity 99.999%
Typical Impurities Lu = 10; Ca, Er, Fe < 5 ppm