MV Labs ZR400 ZrOCl2·xH2O Zirconyl chloride hydrate (low Hf)

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs ZR400 ZrOCl2·xH2O Zirconyl chloride hydrate (low Hf).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 178.13 g/mol
178.13 g/mol
Descriptive Properties Value Comments
Assay 36% Zr
CAS Number 15461-27-5
Form White powder
Purity 99.99+%
Typical Impurities Hf = 30; Al, < 5; Ca, Fe, Mg < 1 ppm