Mallard Creek Polymers BarrierPro® 4551 Styrene-Butadiene Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name BarrierPro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers BarrierPro® 4551 Styrene-Butadiene Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Barrier Pro® 4551 is a carboxylated styrene-butadiene emulsion with excellent strength properties, high resistance to liquid water and water vapor, high blush resistance and excellent adhesion to multiple construction substrates. Barrier Pro® 4551 has excellent stability with dry-add inorganic fillers and sets quickly into a low tack, high strength, water resistant film. Barrier Pro® 4551 is also a good base polymer for blending with other Barrier Pro® products to allow a membrane to be custom tailored to a specific strength and/or flexibility need. Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Barrier Pro® 4551 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 52.5 - 54.5 %
52.5 - 54.5 %
pH 7.0 - 8.0
7.0 - 8.0
Brookfield Viscosity <= 1000 cP
<= 1000 cP
#20/200
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 10.0 °C
50.0 °F
Descriptive Properties Value Comments
Emulsifiers Anionic