Mallard Creek Polymers ROVENE® 18106 Styrene-Acrylic Emulsion

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Mallard Creek Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mallard Creek Polymers ROVENE® 18106 Styrene-Acrylic Emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ROVENE® 18106 is a styrene-acrylic copolymer emulsion. This latex provides good water resistance together with good grease resistance. ROVENE® 18106 exhibits excellent mechanical stability and can be applied to a variety of substrates using various application methods. REGULATORY STATUS: FDA compliant for food contact-176.170 components of paper and paperboard in contact with aqueous and fatty foods, 176.180 components of paper and paperboard in contact with dry food. Kosher approved polymer. STORAGE AND HANDLING Protect from freezing. Ideal storage temperature is 22°C (72°F). Stability at 22°C (72°F) is 180 days when properly stored. Read the ROVENE® 18106 Material Safety Data Sheet before handling, storing, or using this product.APPLICATIONS: ROVENE® 18106 typical applications are for use in clear barrier coatings for paper and paperboard. Other uses include nonwoven saturation by a variety of applications methods such as dip/nip or spray.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 51 - 53 %
51 - 53 %
Particle Size 0.20 µm
0.20 µm
pH 7.0 - 7.5
7.0 - 7.5
Brookfield Viscosity <= 400 cP
<= 400 cP
#2/20 rpm
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 10.0 °C
50.0 °F
Descriptive Properties Value Comments
Emulsifiers Nonionic
Residual Monomer 0.07% Max
Users viewing this material also viewed the following: