Master Bond X-5 Elastomer Based, One Component Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond X-5 Elastomer Based, One Component Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond X-5 is specially formulated, synthetic elastomer-based, one component adhesive for high performance bonding and sealing. This synthetic elastomer based adhesive bonds well in both shear and peel to similar and dissimilar surfaces including metals, woods, most plastics, ceramics, glass, rubber, paper, leather, wallboard and insulation, concrete, plastic foams and stone.
Physical Properties Metric English Comments
Solids Content 30 %
30 %