Mateck NdCaAlO4

Category Ceramic , Oxide
Manufacturer Mateck GmbH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck NdCaAlO4.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Substrate single crystals for superconductivity
Physical Properties Metric English Comments
a Lattice Constant 3.685 Ã…
3.685 Ã…
c Lattice Constant 12.12 Ã…
12.12 Ã…
Thermal Properties Metric English Comments
Melting Point 1850 °C
3360 °F
Electrical Properties Metric English Comments
Dielectric Constant 19.5
19.5
Descriptive Properties Value Comments
Growth Techniques Czochralski
Structure tetragonal