Mateck SrTiO3

Category Ceramic , Oxide , Titanium Oxide
Manufacturer Mateck GmbH
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck SrTiO3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Substrate bicrystals for superconductivity
Physical Properties Metric English Comments
a Lattice Constant 3.905 Ã…
3.905 Ã…
Thermal Properties Metric English Comments
CTE, linear 11.1 µm/m-°C
6.17 µin/in-°F
Melting Point 2080 °C
3780 °F
Electrical Properties Metric English Comments
Dielectric Constant 310
310
Descriptive Properties Value Comments
Dimensions (mm) 10x10x0.5
Junction Angle ° 24±1
36.8±1
Phase Transition Temperature (K) max 110
Tetragonal
Structure cubic
Surface Orientation ° 100±1
Surface Roughness (angstroms) 10
max 30