Substrate single crystals for superconductivity
Physical Properties Metric English Comments
a Lattice Constant 5.125 Ã…
5.125 Ã…
Thermal Properties Metric English Comments
CTE, linear 8.00 µm/m-°C
4.44 µin/in-°F
Melting Point 2780 °C
5040 °F
Electrical Properties Metric English Comments
Dielectric Constant 27
27
Descriptive Properties Value Comments
Flatness (µm/10mm), max 1
Growth Techniques Flux
Orientation (100)
Orientation Accuracy ( ° ), Max 0.5
Parallelness ( ° ), max 0.02
Polishing standard: one side epi-polished
Production Method Skull method
Roughness of surface (angstroms), max 40
Scratches none
Standard Size (mm) 10 x 10 x 0.5
State monocrystalline
Structure cubic
Surface Quality with light microscope without defects