Mateck ZnO

Category Ceramic , Oxide
Manufacturer Mateck GmbH
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mateck ZnO.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Substrate single crystals for III-V nitrides
Physical Properties Metric English Comments
a Lattice Constant 3.325 Ã…
3.325 Ã…
c Lattice Constant 5.213 Ã…
5.213 Ã…
Thermal Properties Metric English Comments
Melting Point 1975 °C
3587 °F
Descriptive Properties Value Comments
Growth Techniques Hydrothermal
Lattice Mismatch to GaN 2.2
Orientation (0001)
Orientation Accuracy ( ° ), Max 30
Polishing one side or both sides epi-polished
Standard Size (mm) 10 x 10, 10 x 5, thickness 0.4 mm
State monocrystalline
Structure hexagonal
Tolerance of Length (mm) 0.05