Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mearthane Durethaneâ„¢ M DM-630A Foam Polyurethane

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Mearthane Products Corporation (MPC)
Trade Name Durethane™ M
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mearthane Durethaneâ„¢ M DM-630A Foam Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MDI backbone: ester.Shore 00 Hardness: 75Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Durethane M is very economical, and has excellent resistance to compression set. It can be formulated to form an integral skin.Applications: The compression set resistance of Durethane M makes it an effective material for applications with repeated compression cycles, such as actuator pads on postal meters and idler belts.Conductivity: All Durethane elastomers can be formulated to be electrically conductive, for applications involving electrostatic dissipation (ESD). Mearthane's proprietary conductivity process does not comprise the material performance specification of the urethane.Information provided by Mearthane Products Corporation.
Physical Properties Metric English Comments
Density 0.480 g/cc
0.0173 lb/in³
ASTM D3574A
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
ASTM D2240
Tensile Strength, Ultimate 48.6 MPa
7050 psi
ASTM D3574E
Elongation at Break 525 %
525 %
ASTM 3457E
100% Modulus 0.00100 GPa
0.145 ksi
ASTM D3574E
200% Modulus 0.00117 GPa
0.170 ksi
ASTM D3574E
300% Modulus 0.00190 GPa
0.276 ksi
ASTM D3574E
Compressive Yield Strength 0.240 MPa
34.8 psi
at 10% deflection; ASTM D3574C
0.410 MPa
59.5 psi
at 20% deflection; ASTM D3574C
0.660 MPa
95.7 psi
at 30% deflection; ASTM D3574C
Resilience 33
33
Bashore Rebound; ASTM 2632D
Tear Strength Test 80
80
lb; Die C; ASTM 3457F
Users viewing this material also viewed the following: