Material Notes:
Description: Repulpable water resistant paper coatingUsage: HydraBan® 708 is an economical, water based treatment for kraft paper. It imparts a high degree of water repellency, is printable and gluable. It can be applied at the wet end or dry end of the corrugator, or with an off-line treating operation.Application data: HydraBan® 708 may be applied at the corrugator by blade or rod and may also be spray applied.HydraBan® is typically used for: Produce boxes; Outdoor storage and Home improvement productFood Contact Information when manufactured in the USA and Belgium: FDA: 175.105: Components of adhesives 176.170: Components of paper and paperboard in contact with aqueous and fatty foods176.180: Components of paper and paperboard in contact with dry foods.When manufactured in Belgium product meets food contact regulations for: Europe: Euro. Res. AP(2004)1(Restricted) Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)Food Contact Information when manufactured in Singapore: FDA: 175.105: Components of adhesives. 175.320: Resinous and polymeric components of coatings for polyolefin films.176.170: Components of paper and paperboard in contact with aqueous and fatty foods176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.930 - 0.950 g/cc
0.930 - 0.950 g/cc
pH 10 - 11
10 - 11
Brookfield Viscosity <= 600 cP
<= 600 cP
Spindle # 3, rpm 60
Viscosity Measurement 15 - 30
15 - 30
[sec], EZ cup, Cup # 2
Descriptive Properties Value Comments
Appearance White liquid
Solids Type Scale