Michelman® Hydrosize® HP-1632 Polyimide solution

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Hydrosize®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Hydrosize® HP-1632 Polyimide solution.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyimide solutionHydrosize® HP-1632 is a specialty coating and high temperature fiber sizing with excellent adhesion properties and abrasion resistance.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Volatiles 88 - 90 %
88 - 90 %
pH 7.5 - 10.5
7.5 - 10.5
Brookfield Viscosity <= 8000 cP
<= 8000 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance Transparent yellow-brown liquid
Solids Type Polyimide