Material Notes:
Description: Styrene-Acrylate copolymer dispersion, metal containingUsage: Licomer® M 55 is an aqueous polymer dispersion for the manufacture of dry-bright emulsions intended especially for the care of floors. This product provides high gloss, good traffic resistance, good dirt repellence and low presence of black heel marks, easy removal with ammonium cleaning agents, and excellent water and detergent resistance.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.06 - 1.08 g/cc
1.06 - 1.08 g/cc
Volatiles 61 - 63 %
61 - 63 %
pH 8.0 - 9.5
8.0 - 9.5
Brookfield Viscosity <= 140 cP
<= 140 cP
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Milky white liquid
Emulsifier Charge Anionic/Nonionic
Solids Type Styrene Acrylate Copolymer