Michelman® Licomer® W 483 Nonionic montan emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Licomer®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Licomer® W 483 Nonionic montan emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic montan emulsionUsage: Licomer® W 483 is a high gloss concentrated emulsion, used for dry-bright polishes.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.02 g/cc
1.00 - 1.02 g/cc
Volatiles 69 - 71 %
69 - 71 %
pH 3.5 - 5.5
3.5 - 5.5
Brookfield Viscosity <= 140 cP
<= 140 cP
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance White liquid
Emulsifier Charge Nonionic
Solids Type Montan