Michelman® Michem® Emulsion 13025 Slip and anti-block additive

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 13025 Slip and anti-block additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Slip and anti-block additiveUsage: Michem® Emulsion 13025 provides slip and block resistance in a wide variety of coatings and formulas. It has a very broad global food contact compliance, combined with a wide pH compatibility.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamFood Contact Information when manufactured in the USA:FDA:175.105: Components of adhesives.175.300: Resinous and polymeric components of coatings. 175.320: Resinous and polymeric components of coatings for polyolefin films. 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. 176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 74.5 - 75.5 %
74.5 - 75.5 %
pH 3.0 - 8.0
3.0 - 8.0
2.0 - 12
2.0 - 12
Recommended pH of system
Brookfield Viscosity <= 40 cP
<= 40 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Tan, low viscosity liquid
Emulsifier Charge Nonionic
Solids Type Carnauba