Michelman® Michem® Guard 60 Nonionic Fischer-Tropsch dispersion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Guard
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Guard 60 Nonionic Fischer-Tropsch dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic Fischer-Tropsch dispersionUsage: Michem® Guard 60 is a dispersion which provides mar resistance properties when used as an additive in paint, coating, ink and graphic art formulations.Typical uses include: Inks and OPVs; Exterior wood and wood composites and Interior furniture and flooringFood Contact Information when manufactured in Belgium:FDA:175.105: Components of adhesives.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
Volatiles 46 - 48 %
46 - 48 %
pH 4.0 - 8.0
4.0 - 8.0
2.0 - 12
2.0 - 12
Recommended pH of system
Brookfield Viscosity 500 - 1000 cP
500 - 1000 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance White, viscous liquid
Emulsifier Charge Nonionic
Solids Type Fischer-Tropsch