Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Michelman® Michem® Tite 335AF Skin packing / heat seal coating

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Tite
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Tite 335AF Skin packing / heat seal coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Skin packing / heat seal coatingUsage: Michem® Tite 335AF is a coating which bonds corrugated to Surlyn or polyethylene skin pack films, firmly trapping the product in between. Adhesion to most water based or litho inks is excellent, but the inks must be wax-free. This product is hot melt gluable. Application Data: Michem® Tite 335AF should be applied to sheeted corrugated using a roll coater.Typical uses include: Displays; Parts packs and Shipping protectionFood Contact Information when manufactured in the USA: FDA:176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
pH 7.8 - 8.8
7.8 - 8.8
Brookfield Viscosity 150 - 850 cP
150 - 850 cP
Spindle # 3, rpm 60
Viscosity Measurement 20 - 45
20 - 45
[sec], EZ cup, Cup # 3
Descriptive Properties Value Comments
Appearance Semi-viscous liquid
Solids Type Polymer