Microcell Composite Company CELLOMER® S-2140 SBS Rubber Foam

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Microcell Composite Company
Trade Name CELLOMER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Microcell Composite Company CELLOMER® S-2140 SBS Rubber Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by Microcell Composite Company
Physical Properties Metric English Comments
Density 0.380 - 0.420 g/cc
0.0137 - 0.0152 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 37 - 41
37 - 41
ASTM D2240
Tensile Strength, Yield 0.981 MPa
142 psi
ASTM D412
Elongation at Yield 250 %
250 %
ASTM D412
Tear Strength 5.88 kN/m
33.6 pli
ASTM D624
Compression Set 65 %

@Temperature 70.0 °C,
Time 21600 sec
65 %

@Temperature 158 °F,
Time 6.00 hour
50%; ASTM D395
Thermal Properties Metric English Comments
Shrinkage 3.0 %

@Temperature 70.0 °C,
Time 2400 sec
3.0 %

@Temperature 158 °F,
Time 0.667 hour
ASTM D1204
Descriptive Properties Value Comments
Resiliency (%) 70
ASTM D2632
Users viewing this material also viewed the following: