Micropol E332 Rotational molding powder based on a random EVA copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Micropol Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol E332 Rotational molding powder based on a random EVA copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ASTM D2240
Tensile Strength, Yield 11.7 MPa
1700 psi
ASTM D638
Elongation at Break 800 - 1000 %
800 - 1000 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 65.0 °C
149 °F
Ring & Ball Softening Point 110 °C
230 °F
ASTM E 28