Minelco Bentonites

Category Ceramic , Clay , Oxide , Silicon Oxide
Manufacturer Minelco Inc.
Trade Name Bentonites
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Minelco Bentonites.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A range of natural sodium, soda activated or calcium cation montmorillonite clays.Applications: Foundry Greensand Binder & AdditiveHorizontal Directional and Vertical DrillingSoil/Landfill and Drillhole SealantsCivil, Construction and Foundation EngineeringPaper Processing and Water TreatmentGeneral Plasticizer, Viscosifier and Suspension AgentConsumer and Industrial AbsorbentsPalletizing
Component Elements Properties Metric English Comments
Al2O3 16.1 %
16.1 %
Fe2O3 2.3 %
2.3 %
K2O 4.5 %
4.5 %
Montmorillonite 80 - 90 %
80 - 90 %
SiO2 54.8 - 63.2 %
54.8 - 63.2 %
Sulfur, S 24.8 %
24.8 %
Descriptive Properties Value Comments
Appearance White, beige or grey powder and granules
Cation Exchange Capacities, meq/100g 93 to 109