Material Notes:
Highly flexible, non-abrasive, chemical-resistant PTFE coating with very good easy-to-clean properties, biocompatible.Information provided by Möller Medical, Member of CENTROTEC Group
Physical Properties Metric English Comments
Thickness 10.0 - 30.0 microns
0.394 - 1.18 mil
Mechanical Properties Metric English Comments
Taber Abrasion, mg/1000 Cycles 21
21
CS17 friction disc with 500g load; DIN 53754
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Processing Properties Metric English Comments
Processing Temperature 340 - 400 °C
644 - 752 °F
Hardening Temperature
Descriptive Properties Value Comments
Applicable Substrate Aluminum
Copper
Glass
with restrictions
Stainless Steel
Biocompatibility Biocompatible
One-parametric cytotoxicity test
Contact Angle to Water [deg] 103
Cupping Test [mm] 8.3
DIN EN ISO 1520
Non-Applicable Substrate ABS
Brass
Nylon
PMMA
Polycarbonate
Tubes int. dia. 0.1-10 mm
Pendulum Dampening Test [sec] 120-140
DIN EN ISO 1522