Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials RTV118 Translucent Adhesive Sealant, General Purpose Pourable

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV118 Translucent Adhesive Sealant, General Purpose Pourable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: Thin-section protective coating; seal, bond, insulate, and encapsulate.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
Tensile Strength, Ultimate 2.20 MPa
319 psi
Elongation at Break 325 %
325 %
Adhesive Bond Strength 0.830 MPa
120 psi
Typical lap shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 205 °C
401 °F
Continuous useful temperature.
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Continuous useful temperature.
Electrical Properties Metric English Comments
Dielectric Constant 2.8

@Frequency 60 Hz
2.8

@Frequency 60 Hz
Dielectric Strength 15.6 kV/mm
396 kV/in
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Users viewing this material also viewed the following: