Momentive Performance Materials RTV6445 Heat-Curing Silicone Adhesive, White

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials RTV6445 Heat-Curing Silicone Adhesive, White.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
RTV6424, RTV6445, and TSE322 silicone adhesives are one-component heat curable silicone adhesive sealants which will bond to many substrates without a primer and which will creep rapidly at elevated temperatures. These products have a very long working time at room temperature but will not cure completely until exposed to elevated temperatures. RTV6445 is a white, thixotropic paste consistency product which can be applied to vertical or overhead surfaces.Mechanical properties for specimen cured 1 hour at 150°C.Key Performance Properties: One component product - no mixing requiredFast cure at elevated temperaturePrimerless adhesion to many types of substratesNo cure by-products, low linear shrinkageExcellent dielectric propertiesOutstanding performance over a wide thermal range.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
Tensile Strength, Ultimate 6.033 MPa
875.0 psi
Elongation at Break 625 %
625 %
Adhesive Bond Strength 2.24 MPa
325 psi
Aluminum to aluminum
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Constant 2.9
2.9
Dielectric Strength 19.69 kV/mm
500.1 kV/in
Dissipation Factor 0.0030
0.0030
Descriptive Properties Value Comments
Application rate 50 g/min
Color White
Vertical flow 0.2 inches
at 5 minutes