Material Notes:
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, GoodWeldable Forms:PelletsProcessing Method:Extrusion Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM 792
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
10 seconds; ASTM D2240
Tensile Strength, Yield 5.52 MPa
800 psi
Elastic; ASTM D412
Elongation at Break 600 %
600 %
Elastic; ASTM D412
Tear Strength 19.3 kN/m
110 pli
ASTM D624
Compression Set 13 %
13 %
73°F, 70 hours; ASTM D395
24 %
24 %
158°F, 70 hours; ASTM D395
Processing Properties Metric English Comments
Die Temperature 204 °C
400 °F
Melt Temperature 191 - 204 °C
375 - 400 °F