Multibase Multi-Flex® A 6221 TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 6221 TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Chemical Resistance, Good Thermal Stability, GoodOzone ResistantGeneral PurposeForms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsAutomotive Under the HoodInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM 792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 16 g/10 min

@Load 2.16 kg,
Temperature 230 °C
16 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
10 seconds; ASTM D2240
Tensile Strength, Yield 1.31 MPa
190 psi
at 100%; ASTM D638
3.79 MPa
550 psi
Elastic; ASTM D638
Elongation at Break 650 %
650 %
Elastic; ASTM D638
Tear Strength 21.0 kN/m
120 pli
ASTM D624
Compression Set 26 %
26 %
73°F, 70 hours; ASTM D395
76 %
76 %
158°F, 70 hours; ASTM D395