Multibase Multi-Flex® A 7727 E Black TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 7727 E Black TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
ASTM 792
Melt Flow 1.45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
10 seconds; ASTM D2240
Tensile Strength, Yield 5.52 MPa
800 psi
Elastic; ASTM D412
Elongation at Break 600 %
600 %
Elastic; ASTM D412
Tear Strength 38.6 kN/m
220 pli
ASTM D624
Compression Set 72 %
72 %
158°F, 22 hours; ASTM D395