Multibase Multi-Flex® TPE A 7020 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 7020 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.229 g/cc
0.04440 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
10 sec; ASTM D-2240
Tensile Strength, Ultimate 3.50 MPa
508 psi
ASTM D412
Elongation at Break 696 %
696 %
ASTM D412
Flexural Modulus 0.0279 GPa
4.05 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 25.2 kN/m
144 pli
ASTM D624