Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPO 4308 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO 4308 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955-89
Melt Flow 8.0 g/10 min
8.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate >= 10.13 MPa
>= 1469 psi
ASTM D638-95
Elongation at Break 310 %
310 %
ASTM D638-95
Flexural Modulus 0.206 - 0.344 GPa
29.9 - 49.9 ksi
Secant 1%; ASTM D-790-95
Tear Strength 81.6 kN/m
466 pli
ASTM D624-95