Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPO D 5308 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D 5308 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955-89
Melt Flow 8.0 g/10 min
8.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 10.0 MPa
1450 psi
ASTM D638-95
Elongation at Break >= 350 %
>= 350 %
ASTM D638-95
Elongation at Yield 22 %
22 %
ASTM D638-95
Flexural Modulus 0.548 GPa
79.5 ksi
Secant 1%; ASTM D-790-95
Izod Impact, Notched NB
NB
ASTM D-256-93a
Tear Strength 98.0 kN/m
559 pli
ASTM D624-95